项  目 | 100 | 150 | 200 | 250 | 300 | 350 | 400 | 450 | 500 | 600 | 800 | 备注 |
| 单位面积质量偏差,% | -6 | -5 | -4 | |||||||||
| 厚度,mm,≥ | 0.8 | 1.2 | 1.6 | 1.9 | 2.2 | 2.5 | 2.8 | 3.1 | 3.4 | 4.2 | 5.5 | |
| 幅度偏差,% | -0.5 | |||||||||||
| 断裂强力,KN/m≥ | 4.5 | 7.5 | 10.0 | 12.5 | 15.5 | 17.5 | 20.5 | 22.5 | 25.0 | 30.3 | 40.0 | 纵横向 |
| 断裂伸长率,% | 40-80 | |||||||||||
| CBR顶破强力,KN≥ | 0.8 | 1.4 | 1.8 | 2.2 | 2.6 | 3.0 | 3.5 | 4.0 | 4.7 | 5.5 | 7.0 | |
| 等效孔径090(095),mm | 0.07-0.2 | |||||||||||
| 垂直渗透系数,cm/s | Kx(10-4~10-3),k=1.0-9.9 | K=1.0-9.9 | ||||||||||
| 撕破强力,KN≥ | 0.14 | 0.21 | 0.28 | 0.35 | 0.42 | 0.49 | 0.56 | 0.63 | 0.70 | 0.82 | 1.10 | 纵横向 |
| 聚酯长丝烧毛土工布技术指标 | |||
项  目 | SMFNG160 | SMFNG180 | SMFNG200 |
| 单位面积质量(g/㎡) | 160 | 180 | 200 |
| 厚度(mm) | 1.4 | 1.5 | 1.6 |
| 断裂强度(纵横向)(KN/m>) | 8 | 9 | 10 |
| 断裂伸长率(纵横向)(%) | 40-70 | ||
| 梯形撕破强度(纵横向)(KN>) | 0.23 | 0.26 | 0.28 |
| CBR顶破强度(KN>) | 1.5 | 1.7 | 1.8 |
| 承载强度(KN>) | 20 | 23 | 25 |
| 等效孔径095(mm) | 0.07-0.2 | ||
| 垂直渗透系数(cm/s) | Kx(10-1~10-3),k=1~9.9 | ||
| 幅宽(m) | 4.4 | ||